Polymer Property : Peel Strength = 5.61 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 5.61 kN/m

@Temperature 177 °C
32.0 pli

@Temperature 350 °F
Roller Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D3167
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive
Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character..
Peel Strength 5.61 kN/m

@Temperature 24.0 °C,
Time 605000 sec
32.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 5.61 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
32.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 5.61 kN/m

@Temperature 80.0 °C
32.0 pli

@Temperature 176 °F
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and ..