Mechanical Properties Metric English Comments
Fatigue Strength 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
R=smin/smax=0.1; 2 million cycles, F50
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 320 MPa

@# of Cycles 1.00e+8
40600 - 46400 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200)
Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Fatigue Strength 280 - 310 MPa

@# of Cycles 1.00e+8
40600 - 45000 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Fatigue Strength 280 MPa
40600 psi
test conditions not reported
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..