Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 56.0 MPa @# of Cycles 1.00e+6 |
8120 psi @# of Cycles 1.00e+6 |
10 Hz, ASTM Type I tensile bar |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Fatigue Strength | 56.0 MPa @# of Cycles 1.00e+6 |
8120 psi @# of Cycles 1.00e+6 |
1 Hz |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Fatigue Strength | 56.0 MPa @Frequency 1.00 Hz, # of Cycles 1.00e+6 |
8120 psi @Frequency 1.00 Hz, # of Cycles 1.00e+6 |
ASTM D638 |
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. .. |