Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 660 MPa @# of Cycles 1.00e+7 |
95700 psi @# of Cycles 1.00e+7 |
R.R. Moore Test, Smooth Rotating Beam |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |