Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 123 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 134 PC Nonhalogenated. 3.5 MFR. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 201R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 221 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® OQ4320R PC Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific) Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP2NR PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 950 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |