Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific) LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C.. |
|||
Dart Drop, Total Energy | 3.00 - 29.0 J | 2.21 - 21.4 ft-lb | Average value: 7.04 J Grade Count:27 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12 LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific) LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific) LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold.. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX00887C PC LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific) LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL FN215X PPE+PS Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction. |