Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.127 MPa | 18.4 psi | ASTM D3574E |
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience, Higher density Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |