Polymer Property : Tensile Strength, Ultimate = 1035 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1035 MPa
>= 150100 psi
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Tensile Strength, Ultimate >= 1035 MPa
>= 150100 psi
MetalTek MTEK M-152 Martensitic Stainless Steel
"400" series, General corrosion resistant alloy, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTek..
Tensile Strength, Ultimate 1035 MPa
150100 psi
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1035 MPa
150100 psi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero..
Tensile Strength, Ultimate 1035 MPa
150100 psi
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Tensile Strength, Ultimate 1035 MPa

@Temperature -196 °C
150100 psi

@Temperature -321 °F
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves. Standard, rotor/premium grades.
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® 6-2-4-2-Si UNS R54620 modified Titanium Alloy
Uses: High performance valves for internal combustion engines. Aerospace and commercial grades.Property values are for samples in the metallurgical condition: 1800°F anneal.Information provided by ..
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Fan & compressor blades, discs, spacers, seals, rings. Excellent creep resistance. Standard, rotor/premium grades.
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Jet engines, superchargers, missile components, fasteners, cryogenic equipment, nuclear, corrosive deep well hardware.
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Data provided by Allvac.Applications: High temperature applications, jet engine components, devices in high fatigue service.
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allvac® Vasco® 450 Specialty Steel, Heat Treatment: 1038°C (1900°F) + Age
Data provided by Allvac.Applications: Land-based turbine blades and buckets.
Tensile Strength, Ultimate 1035 MPa
150100 psi
Longitudinal
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..
Tensile Strength, Ultimate 1035 MPa
150100 psi
ATI Allegheny Ludlum AL 15-5 High Strength Stainless Steel, UNS S15500
Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts.Information provided by Allegheny Ludlum
Tensile Strength, Ultimate <= 1035 MPa
<= 150100 psi
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718
Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro..
Tensile Strength, Ultimate 1035 MPa
150100 psi
Kennametal Stellite Stellite® 31 PM after P/M processing, aged 8 hours at 802°C air cooled
Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we..