Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.0 - 138 MPa
3480 - 20000 psi
Average value: 40.4 MPa Grade Count:64
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Tensile Strength, Ultimate 29.0 - 138 MPa
4210 - 20000 psi
Average value: 72.7 MPa Grade Count:55
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Tensile Strength, Ultimate 45.0 - 138 MPa
6530 - 20000 psi
Average value: 93.7 MPa Grade Count:35
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Tensile Strength, Ultimate 65.5 - 138 MPa
9500 - 20000 psi
Average value: 95.2 MPa Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 68.9 - 138 MPa
10000 - 20000 psi
Average value: 115 MPa Grade Count:15
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Tensile Strength, Ultimate 9.28 - 138 MPa

@Temperature -20.0 - 200 °C
1350 - 20000 psi

@Temperature -4.00 - 392 °F
Average value: 49.7 MPa Grade Count:1
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Tensile Strength, Ultimate 9.28 - 138 MPa

@Strain 0.230 - 4.21 %
1350 - 20000 psi

@Strain 0.230 - 4.21 %
Average value: 49.7 MPa Grade Count:1
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Tensile Strength, Ultimate 34.0 - 138 MPa
4930 - 20000 psi
Average value: 76.3 MPa Grade Count:61
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 82.7 - 138 MPa
12000 - 20000 psi
Average value: 95.9 MPa Grade Count:6
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Tensile Strength, Ultimate 48.3 - 138 MPa
7000 - 20000 psi
Average value: 88.2 MPa Grade Count:45
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 86.2 - 138 MPa
12500 - 20000 psi
Average value: 110 MPa Grade Count:12
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..