Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric.. |
|||
Tensile Strength, Ultimate | 165 - 318 MPa | 23900 - 46100 psi | Average value: 245 MPa Grade Count:40 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Tensile Strength, Ultimate | >= 165 MPa | >= 23900 psi | |
MetalTek Bearium® B-8 Bearing Bronze Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mis.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | Annealed |
CMW® D505F Silver Nickel Contact Material For electrical contacts.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | Rm |
ALIMEX ACP 6000 Aluminum Cast Plate Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and .. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
A. Schulman ComAlloy E-16026N Internally Lubricated, Carbon Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 646 Nylon 6/12, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ISO 527-1/-2 |
DSM Arnite® TV4 491 (PBT+PET)-GF50 |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Adell DR-18 40% Glass Reinforced Polycarbonate |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |