Polymer Property : Tensile Strength, Ultimate = 179 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Nylene® 9643 , 43% Glass Reinforced Nylon 6,6/6
Description: Nylene® 9643 is a 43 % glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Reso..
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d..
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET  (discontinued **)
Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins.
Tensile Strength, Ultimate 179 MPa
26000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced  (discontinued **)
Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 179 MPa
26000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® NL-20CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 179 MPa
26000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 179 MPa

@Temperature 982 °C
26000 psi

@Temperature 1800 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone
Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory..
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Strength, Ultimate 179 - 262 MPa
26000 - 38000 psi
Eagle Brass 110 EPT COPPER, Annealed
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Ultimate 179 MPa
26000 psi
Dow Saran® 510 PVDC
SARAN® 510 resin is a copolymer of vinylidene chloride and vinyl chloride, supplied as a white free flowing powder (particle size 250 microns). It is a formulated polymer designed for extrusion int..
Tensile Strength, Ultimate 179 - 262 MPa
26000 - 38000 psi
Eagle Brass 101 OFE COPPER (Certified), Annealed
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Ultimate 179 - 262 MPa
26000 - 38000 psi
Eagle Brass 102 OF COPPER (Non-Certified), Annealed
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Ultimate 179 MPa
26000 psi
annealed
CMW® ELKONIUM 46 Silver Alloy
The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low cont..
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Adell BR-38 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Adell BR-18 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 179 MPa
26000 psi
ATSM D638
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced
A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer
Tensile Strength, Ultimate 179 MPa
26000 psi
ATSM D638
Ashley Polymers Ashlene® 830LS-33G Nylon 6, 33% Glass Reinforced
A 33% glass fiber reinforced and heat stabilized Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 t..
Tensile Strength, Ultimate 179 MPa
26000 psi
10 oz glass cloth laminate
BCC Products BC 5114 Epoxy Laminating System
BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use abov..
Tensile Strength, Ultimate 179 MPa
26000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 179 MPa
26000 psi
ATSM D638
Ashley Polymers Ashlene® 830L-33G Nylon 6, 33% Glass Reinforced
A 33% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p..