Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2100 MPa | 304000 psi | |
Latrobe Marvac 300 VIM-VAR ; 6.25 in. High Strength Maraging Steel MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | |
Cytec Thornel® P-100S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been .. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | |
Cytec Thornel® P-650/35 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | |
Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | hardness of 54 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Tensile Strength, Ultimate | 2100 MPa @Thickness 25.4 mm |
305000 psi @Thickness 1.00 in |
gauge filament |
3M Nextel™ 720 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
Tensile Strength, Ultimate | 2100 MPa | 305000 psi | R<sub>m</sub>. 54 HRC. |
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |