Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 234 MPa | 34000 psi | |
Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE IV, CLASS AAll information provided by Pa.. |
|||
Tensile Strength, Ultimate | 234 MPa | 34000 psi | |
PSM Industries Pacific Sintered Metals Nickel Silver BZN-131-U Powdered Metal Higher strength than brass, Good corrosion resistance Equivalent MPIF Specification: CZN-1818-17Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 234 MPa | 34000 psi | |
Pacific Sintered Materials BZN-131-U Nickel Silver Powdered Metal Higher strength than brass. Good corrosion resistance.Equivalent MPIF Specification: CZN-1818-17All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 234 MPa @Temperature 93.3 °C |
34000 psi @Temperature 200 °F |
Brass butt joint |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Tensile Strength, Ultimate | 234 MPa @Temperature 93.3 °C |
34000 psi @Temperature 200 °F |
Brass butt joint |
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning .. |
|||
Tensile Strength, Ultimate | 234 MPa | 34000 psi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 234 - 290 MPa | 34000 - 42000 psi | |
Eagle Brass 110 EPT COPPER, 1/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 234 - 276 MPa | 34000 - 40000 psi | |
Eagle Brass 210 Gilding Metal, Annealed CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 234 - 290 MPa | 34000 - 42000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), 1/4 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 234 - 290 MPa | 34000 - 42000 psi | |
Eagle Brass 101 OFE COPPER (Certified), 1/4 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 234 MPa | 34000 psi | |
PSM Industries Pacific Sintered Metals Iron F-241-S2 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type IV, Class AInformation Provided by Pacific Sintered Metals, a d.. |
|||
Tensile Strength, Ultimate | 234 MPa @Temperature 927 °C |
33900 psi @Temperature 1700 °F |
|
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |