Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.30 MPa | 479 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 8599 BLK TPE compound for acoustic barrier applications requiring high density. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 3.30 MPa | 479 psi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Tensile Strength, Ultimate | 3.30 MPa | 479 psi | ASTM D412 |
Momentive Performance Materials 1200® Construction Sealant One-part, premium glazing sealant for structural as well as general purpose glazing. Cure Method: Acetoxy. Tack-free time |
|||
Tensile Strength, Ultimate | 3.30 MPa | 479 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8400 Polyolefin Elastomer Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr.. |
|||
Tensile Strength, Ultimate | 3.30 MPa | 479 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8407 Polyolefin Elastomer Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p.. |