Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
Pacific Sintered Materials FC-203-N Copper Iron Powdered Metal Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-1000-20All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
PSM Industries PolyAlloys MIM-Fe-50%Co Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
PSM Industries Pacific Sintered Metals Copper Iron FC-203-N Powdered Metal Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-1000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal Applications: 80-20 leaded brass, coined for close dimensional control, strength and density.Equivalent MPIF Specification: CZP-2000-12All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif.. |
|||
Tensile Strength, Ultimate | 207 - 241 MPa | 30000 - 35000 psi | Copper butt joint |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Tensile Strength, Ultimate | 207 - 241 MPa | 30000 - 35000 psi | Copper butt joint |
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning .. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | |
Meehanite GE-30 Flake Graphite Cast Iron Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Annealed |
CMW® D55X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | annealed |
CMW® ELKONIUM 23 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | annealed |
CMW® ELKONIUM 28 Silver Alloy ELKONIUM® 28, a silver-manganese alloy, was developed by CMW specifically for the control of the transfer of contact material in low voltage DC applications. It is used as a positive contact operat.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | annealed |
CMW® ELKONIUM 63 Silver Alloy ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile volta.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 207 MPa | 30000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |