Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2100 MPa
305000 psi
Cytec Thornel® P-100S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been ..
Tensile Strength, Ultimate 2100 MPa
305000 psi
Cytec Thornel® P-650/35 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Tensile Strength, Ultimate 2100 MPa
305000 psi
Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Tensile Strength, Ultimate 2100 MPa
305000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
Tensile Strength, Ultimate 2100 MPa
305000 psi
hardness of 54 HRC
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are ..
Tensile Strength, Ultimate 2100 MPa
305000 psi
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Tensile Strength, Ultimate 2100 MPa

@Thickness 25.4 mm
305000 psi

@Thickness 1.00 in
gauge filament
3M Nextel™ 720 Composite Ceramic Fiber
Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 ..
Tensile Strength, Ultimate 2100 MPa
305000 psi
R<sub>m</sub>. 54 HRC.
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..