Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 37.9 - 67.0 MPa | 5500 - 9720 psi | Average value: 59.1 MPa Grade Count:7 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | |
Elastomer Engineering E850-85A Polyurethane A very tough and cut-resistant polyether-based formulation with good dynamic properties that bonds well to all metals. Information provided by Elastomer Engineering Inc (EEI) |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Total PPH 3720WZ Polypropylene, Injection Molding Grade High flow reactor injection molding homopolymerHigh Flow - FINA 3720WZ has high flow characteristics that result in ease of filling thin wall parts.Nucleation - FINA 3720WZ is nucleated to provide f.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Total PPH 3721WZ Polypropylene, Injection Molding Grade High flow reactor homopolymer with a high level of antistatHigh Flow - FINA 3721WZ is designed with high flow characteristics for ease of filling thin wall parts.High Antistat - FINA 3721WZ is engin.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 37.9 MPa @Temperature 788 °C |
5500 psi @Temperature 1450 °F |
|
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | |
Dymax 3094 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | cured 30 days @ 25°C |
Abatron AboCast 8110-2/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | |
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
Tensile Strength, Ultimate | 37.9 - 45.5 MPa | 5500 - 6600 psi | Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | after optimum cure |
Armstrong A-1/V Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Tensile Strength, Ultimate | 37.9 - 44.8 MPa | 5500 - 6500 psi | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | |
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D638 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 37.9 - 240 MPa | 5500 - 34800 psi | Average value: 108 MPa Grade Count:88 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D412 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |
|||
Tensile Strength, Ultimate | 37.9 - 124 MPa | 5500 - 18000 psi | Average value: 66.3 MPa Grade Count:25 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | TM R050-36 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | ASTM D412 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |
|||
Tensile Strength, Ultimate | 37.9 MPa | 5500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-10GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |