Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
Multibase Nylex™ 2185 FR V0 Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
Nylene® 4121 (HS) Low Wear Nylon 6/6 Description: Nylene® 4121 (HS) is a high impact, low wear, 2% silicon oil reinforced nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting compani.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
Nylene® Norpex® AX200 Impact Modified Polyphenylene Ether Description: Norpex® AX200 HI Flow is a high impact, high flow Polyphenylene Ether. AX200 is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operti.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
Global ABS-1805 General Purpose ABS
(discontinued **) Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 42.7 MPa @Temperature 23.0 °C |
6190 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene AP102 Acrylonitrile Butadiene Styrene Applications:automotive componentsradiator grillsname platesknobstv componentscosmetic componentselectronic household appliances ectespecially suited for electroplating and painting articles |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
Techmer ES Electrafil® ABS-1251/SD ABS, Static Dissipative Polymer Alloy |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | |
Williams Advanced Alloys WS226A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D412 |
Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane Type: Estane® ALR E77A-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D412 |
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | |
Colorite Polymers 10013G-015 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | |
Dymax 984-LVUF Conformal Coating High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 984-LVUF Conformal CoatingTough, glossy, fluorescing with excellent adhesion to a variety of metal, ceramic and glas.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | |
Dymax Sure Cure™ 984 Conformal Coating High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 984 Sure Cure™ Conformal CoatingTough, glossy fluorescing 2-part system, shadow cures at room temperature. Cure Spe.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638 |
Buckeye Polymers BP ABS 8336 P ABS PlatingABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing a.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | after optimum cure |
Armstrong A-2/W Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | |
BCC Products BC 7009-1 Epoxy Casting BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6200 psi | ASTM D638 |
American Polymers API 392 Polystyrene API 392 is a general purpose polystyrene produced in pellet form for injection molding. API 392 has excellent clarity and high flow.Applications: Used in the manufacture of containers, housewares, .. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638-95 |
Multibase Multi-ABS 3845 Medium Impact ABS Data provided by Multibase. |