Polymer Property : Tensile Strength, Ultimate = 420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.90 MPa
420 psi
Dow Corning SE 9184 WHITE RTV
One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning
Tensile Strength, Ultimate 2.90 MPa
420 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..