Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.0 - 30.0 MPa
2030 - 4350 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer  (discontinued **)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Tensile Strength, Ultimate 14.0 - 30.0 MPa
2030 - 4350 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer  (Unverified Data**)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Tensile Strength, Ultimate 21.0 - 30.0 MPa
3050 - 4350 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Tensile Strength, Ultimate 13.0 - 30.0 MPa
1890 - 4350 psi
Average value: 20.4 MPa Grade Count:7
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 12.0 - 30.0 MPa
1740 - 4350 psi
ATG s.r.l. IR Synthetic Polyisoprene
Tensile Strength, Ultimate 14.0 - 30.0 MPa
2030 - 4350 psi
ATG s.r.l. NR Natural Rubber
Tensile Strength, Ultimate 25.0 - 30.0 MPa

@Temperature 60.0 - 60.0 °C
3630 - 4350 psi

@Temperature 140 - 140 °F
Average value: 28.3 MPa Grade Count:3
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Tensile Strength, Ultimate 10.0 - 30.0 MPa
1450 - 4350 psi
Average value: 22.5 MPa Grade Count:11
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Tensile Strength, Ultimate 15.0 - 30.0 MPa
2180 - 4350 psi
Hydrogenated Nitrile Rubber (HNBR)