Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1378 PRE-ELEC PP 1378 is a conductive thermoplastic compound based on glass-fiber reinforced polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electri.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Rotuba H5 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat re.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **) Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 52.0 MPa @Temperature 23.0 °C |
7540 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Tensile Strength, Ultimate | 52.0 MPa @Temperature 23.0 °C |
7540 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | |
Ineos Styrenics Polystyrene 168M0 (NAFTA) High heat, high molecular weight general purpose polystyrene with low residual volatiles. It is ideally suited for use in critical low taste, low odor food packaging products.Information provided b.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ISO 37 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ISO 37 |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | DIN 53504 |
Lubrizol ESTANE® 58563 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | |
BASF Polystyrol® 165 H Polystyrene (Europe) High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | Static |
Channel Industries 300 Barium Titanate Piezoelectric Modified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devi.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 640 Nylon 6/12, PTFE Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ASTM D638 |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Tensile Strength, Ultimate | 52.0 MPa | 7540 psi | ISO 527 |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |