Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.81 - 52.0 MPa
1420 - 7540 psi
Average value: 24.6 MPa Grade Count:28
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 23.0 - 52.0 MPa

@Temperature 260 - 260 °C
3340 - 7540 psi

@Temperature 500 - 500 °F
Average value: 33.3 MPa Grade Count:4
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Ultimate 24.1 - 52.0 MPa
3500 - 7540 psi
Average value: 36.1 MPa Grade Count:22
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Tensile Strength, Ultimate 20.0 - 52.0 MPa

@Temperature -18.0 - 90.0 °C
2900 - 7540 psi

@Temperature -0.400 - 194 °F
Average value: 35.8 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..