Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.0 - 36.0 MPa
1890 - 5220 psi
Average value: 26.0 MPa Grade Count:91
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Tensile Strength, Ultimate 25.0 - 36.0 MPa
3630 - 5220 psi
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Tensile Strength, Ultimate 25.0 - 36.0 MPa
3630 - 5220 psi
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.