Polymer Property : Tensile Strength, Ultimate = 52200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 360 MPa
39200 - 52200 psi
ArcelorMittal 02 High formability steel for drawing, Cold rolled
Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru..
Tensile Strength, Ultimate 280 - 360 MPa
40600 - 52200 psi
ArcelorMittal 03 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC01) and electroglavanized (DC01+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product..
Tensile Strength, Ultimate 300 - 360 MPa
43500 - 52200 psi
ArcelorMittal 180 BH Bake hardening steel, Cold rolled
Available in the following: uncoated (HC180B), electroglavanized (HC180B+ZE) and Extragal®/Galvannealed (HC180BD+Z)Description: The composition and processing of these steels are designed to promot..
Tensile Strength, Ultimate 270 - 360 MPa
39200 - 52200 psi
ArcelorMittal 52 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX52D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..
Tensile Strength, Ultimate 280 - 360 MPa
40600 - 52200 psi
ArcelorMittal 53 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX53D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..