Polymer Property : Tensile Strength, Ultimate = 5660 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.0 - 39.0 MPa
4790 - 5660 psi
Average value: 37.0 MPa Grade Count:3
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 8.00 - 39.0 MPa
1160 - 5660 psi
Average value: 17.0 MPa Grade Count:18
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
Tensile Strength, Ultimate 22.0 - 39.0 MPa
3190 - 5660 psi
Average value: 31.6 MPa Grade Count:18
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 1.00 - 39.0 MPa

@Temperature 50.0 - 100 °C
145 - 5660 psi

@Temperature 122 - 212 °F
Average value: 14.6 MPa Grade Count:6
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 1.00 - 39.0 MPa

@Strain 20.0 - 20.0 %
145 - 5660 psi

@Strain 20.0 - 20.0 %
Average value: 14.6 MPa Grade Count:6
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 11.0 - 39.0 MPa
1600 - 5660 psi
Average value: 24.5 MPa Grade Count:9
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..
Tensile Strength, Ultimate 29.0 - 39.0 MPa
4210 - 5660 psi
ISO 527
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..