Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D638 |
Novatec Novaloy® 9000 PVC + ABS Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characte.. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D638 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Tensile Strength, Ultimate | 42.2 MPa @Temperature 23.0 °C |
6120 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene AN450 Acrylonitrile Butadiene Styrene Applications:injection moldingelectric/electonic housing for microwave oven, tv, vcr, computer, etc. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D412 |
SK Chemicals SKYTHANE® 155D R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D412 |
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D638 |
SK Chemicals SKYTHANE® SG100 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D412 |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D412 |
Lubrizol Estane® S398A Thermoplastic Polyurethane Type: Estane® S398A is a Shore 98A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Tensile Strength, Ultimate | 42.2 MPa | 6120 psi | ASTM D412 |
Lubrizol Estane® R195A Thermoplastic Polyurethane Type: Estane® R195A is a Shore 95A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |
|||
Tensile Strength, Ultimate | 42.2 MPa @Temperature 23.0 °C |
6120 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets |