Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Plaskolite Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM Data |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Covestro Makrolon® DP1-1243 Polycarbonate, Extrusion
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
IDI Composites 44-10 HGM Thermoset Polyester, Molding Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
IDI Composites A-203 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
IDI Composites C-105 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
IDI Composites C-204 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
LG Chemical Lupoy 1201-18 Polycarbonate Resin Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | |
Haysite 43000 Polyester SMC, 22% Glass Reinforced The 43000 series sheet molding compound is a general purpose material. Designed for compression molding, this grade exhibits good mechanical properties and resistance to mild corrosive agents. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | |
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2) A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | |
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | |
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM Data |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ATSM D638 |
Ashley Polymers Ashlene® P1410 Polycarbonate, 10% Glass Reinforced A 10% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1413: with UV stabilizer.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 69.0 MPa @Temperature 982 °C |
10000 psi @Temperature 1800 °F |
ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Adell DS-10 General Purpose Polycarbonate |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ATSM D638 |
Ashley Polymers Ashlene® 630BU Nylon 6 Black utility grade Nylon 6 for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Chem Polymer Formax 605 G Acetal, 5% Glass Reinforced A lubricated, 5% glass reinforced acetal offering a balance of rigidity, dimensional stability and tensile strength.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 69.0 MPa @Temperature 120 °C |
10000 psi @Temperature 248 °F |
ISO 527 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ISO 527-1, 2 |
Polyplastics Duracon® HP270X Acetal Co-polymer (POM), High stiffness, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
Rostone Rosite® 4030FS SMC Thermoset Polyester, 30% Glass Reinforced
(discontinued **) Key Features: "Zero Shrink" Grade±1/4 mil shrinkage. Provides surface smoothness for uses such as auto headlamp retainers. High impact and flexural strength combined with dimensional accuracy.Inf.. |