Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 724 MPa | 105000 psi | (Tensile Yield Strength near U.T.S.) |
Kennametal Stellite Stellite® 19 Can be machined with carbide tipped tools, but when hardness exceeds Rc55 it is best to grind. Applications include cutting tools, bearing races, guide rolls, and nozzle discs. Excellent resistance .. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Centrifugal Cast 0.250" - 1.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Continuous Cast 0.250" - 4.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Ultimate | >= 724 MPa | >= 105000 psi | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Materion BrushBronze® 630 (AMS 4640) 2.0" - 3.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Ultimate | >= 724 MPa | >= 105000 psi | |
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 724 MPa @Temperature 93.0 °C |
105000 psi @Temperature 199 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Haynes Multimet® alloy, SMAW, 9.5 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Schmolz + Bickenbach MoldMAX® SC Copper Alloy Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot .. |
|||
Tensile Strength, Ultimate | 724 - 820 MPa | 105000 - 119000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 724 - 827 MPa | 105000 - 120000 psi | |
Eagle Brass 70265 XP175, 3/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | Typical; Annealed Plate |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
ATI Allvac® Allcorr® UNS N06110 Nickel Superalloy Uses: Equipment for deep sour gas wells, flue gas desulfurization, chemical and hydrocarbon processing, and pulp and paper.Property values are for samples in the metallurgical condition: 2050°F ann.. |
|||
Tensile Strength, Ultimate | 724 MPa | 105000 psi | |
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems. |
|||
Tensile Strength, Ultimate | 724 MPa @Temperature 93.0 °C |
105000 psi @Temperature 199 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |