Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.0 MPa
7400 psi
DIN 53455; ASTM D638
Kolon SPELLOY® KA101 PC + PBT Alloy Resin  (discontinued **)
SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 51.0 - 69.0 MPa
7400 - 10000 psi
Average value: 58.0 MPa Grade Count:10
Overview of materials for Phenolic, Resole, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Kuraray HYBRAR® PS3 Thermoplastic Rubber-Polystyrene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
LyondellBasell Higlass SB224-2 Polypropylene Copolymer, 20% Glass Fiber
Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, moderate rigidity, good processabilityApplications: of..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 1501 Polyester, Briquette, Transfer Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 2408 Phenolic, Granular, Compression Molded
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 3303 Phenolic, Granular, Compression Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Tensile Strength, Ultimate 51.0 MPa

@Temperature -20.0 °C
7400 psi

@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Toyobo A1071D Thermoplastic Polyurethane Elastomer, Injection Grade
Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ISO 37
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Elastomer Engineering E60D Polyurethane
A polyester-based urethane with particularly high load-bearing characteristics. Information provided by Elastomer Engineering Inc (EEI)
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ISO 527-1, 2
Polyplastics Duranex® 652SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Eastman DURASTAR DS1010 Natural PCTA Copolyester
DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to ..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Eastman Eastar Copolyester BR003, Natural PCTA Copolyester
EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabiliti..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboWeld 48-14/AboCure 48-14 Adhesive/Casting Resin
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboWeld 48-8/AboCure 48-8 Adhesive/Casting Resin
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin
STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 37-10/AboCure 37-10 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 45-10/AboCure 45-10 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 53-15/AboCure 53-15 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Tensile Strength, Ultimate 51.0 - 240 MPa
7400 - 34800 psi
Average value: 148 MPa Grade Count:161
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
XY; ASTM D638
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer
40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ISO 527B
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade  (discontinued **)
Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti..
Tensile Strength, Ultimate 51.0 MPa
7400 psi
5 mm/min; parallel to flow; ASTM D638
Asahi Kasei Tenac®-C EF750 Acetal Copolymer, Antistat  (discontinued **)
Antistatic grade containing special carbon black.Applications: Parts requiring antistatic properties.This product is not a part of the standard product line dated 2003.
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Plenco 2311 Phenolic, Granular, Transfer Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
Tensile Strength, Ultimate 51.0 MPa

@Temperature 120 °C
7400 psi

@Temperature 248 °F
ISO 527
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..