Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 7980 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 55.0 MPa

@Temperature 60.0 - 120 °C
2900 - 7980 psi

@Temperature 140 - 248 °F
Average value: 38.3 MPa Grade Count:1
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Tensile Strength, Ultimate 20.0 - 55.0 MPa

@Temperature 160 - 160 °C
2900 - 7980 psi

@Temperature 320 - 320 °F
Average value: 67.6 MPa Grade Count:2
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Strength, Ultimate 20.0 - 55.0 MPa

@Strain 1.00 - 2.00 %
2900 - 7980 psi

@Strain 1.00 - 2.00 %
Average value: 67.6 MPa Grade Count:2
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Strength, Ultimate 19.0 - 55.0 MPa
2760 - 7980 psi
Average value: 47.8 MPa Grade Count:18
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Ultimate 25.0 - 55.0 MPa

@Temperature 60.0 - 150 °C
3630 - 7980 psi

@Temperature 140 - 302 °F
Average value: 38.4 MPa Grade Count:2
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Ultimate 41.0 - 55.0 MPa
5950 - 7980 psi
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Tensile Strength, Ultimate 41.0 - 55.0 MPa
5950 - 7980 psi
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Tensile Strength, Ultimate 35.0 - 55.0 MPa

@Temperature 60.0 - 120 °C
5080 - 7980 psi

@Temperature 140 - 248 °F
Average value: 43.3 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Tensile Strength, Ultimate 50.0 - 55.0 MPa

@Temperature 160 - 160 °C
7250 - 7980 psi

@Temperature 320 - 320 °F
Average value: 78.5 MPa Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Tensile Strength, Ultimate 50.0 - 55.0 MPa

@Strain 1.00 - 1.70 %
7250 - 7980 psi

@Strain 1.00 - 1.70 %
Average value: 78.5 MPa Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Tensile Strength, Ultimate 41.0 - 55.0 MPa
5950 - 7980 psi
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Tensile Strength, Ultimate 41.0 - 55.0 MPa
5950 - 7980 psi
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Tensile Strength, Ultimate 44.0 - 55.0 MPa
6380 - 7980 psi
Average value: 50.6 MPa Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..