Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 930 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 930 - 1040 MPa
135000 - 151000 psi
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 930 MPa
135000 psi
Haynes 25 alloy, sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 930 MPa
135000 psi
Haynes 556® alloy, 30% cold reduction, 1010°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 930 MPa
135000 psi
Haynes 556® alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 930 MPa
135000 psi
Haynes 625 alloy, 20% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Ultimate 930 MPa
135000 psi
Typical
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
Tensile Strength, Ultimate >= 930 MPa
>= 135000 psi
Typical
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy
Weldable, High Strength, High Temperature, Creep Resistant AlloyFeatures: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIME..
Tensile Strength, Ultimate 930 MPa
135000 psi
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Tensile Strength, Ultimate 930 - 1030 MPa
135000 - 149000 psi
CLAL-MSX NICLAFOR® 1000 TH2 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 930 MPa
135000 psi
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Tensile Strength, Ultimate 930 - 999 MPa
135000 - 145000 psi
Ametek AM 388™ Alloy (UNS C72650) TS02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Ultimate >= 930 MPa
>= 135000 psi
MetalTek MTEK H46 Martensitic Stainless Steel
"400" series, General corrosion resistant alloy, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTek..
Copyright © lookpolymers.com All Rights Reserved