Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 645 MPa @Temperature 540 °C |
93500 psi @Temperature 1000 °F |
|
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |