Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.73 MPa | 976 psi | Cured 7 days at 25°C and 50% relative humidity |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |