Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 1120 g | 1120 g | Method B; ASTM D1922 |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |