Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM D 1922 |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM D1922 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM D1922 |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | |
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. .. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM D1922 |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM D1922 |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | gF; ASTM D1922 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | gF; ASTM D1922 |
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability... |
|||
Elmendorf Tear Strength TD | 520 g | 520 g | ASTM-D1922 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |