Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Dart Drop | 3.95 g/micron | 100 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Westlake EF412 Low Density Polyethylene WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Westlake EF421 Low Density Polyethylene WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | Cast Film at 2.0 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 2121 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: Good processabilityGood drawdownEdge tear resistanceLow neck-in Applications: Typical cast film applicatio.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | 2" Dart, 60" Drop Height; ASTM D1709 |
Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin Resin Type: HomopolymerCharacteristics: Superior tensile and impact strengthGood abrasion and tear resistanceExcellent retention of properties after agingApplications: LaminationsPallet shrinkcase s.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
ExxonMobil LL 1001x26 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop | 3.95 g/micron | 100 g/mil | ASTM-D1709 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | F<sub>50</sub>; ASTM D-1709 |
Bapolene® 107A Low Density Polyethylene Film Extrusion Resin Bapolene® 107A is an LDPE for blown film. It contains 3400 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Dart Drop | 3.94 g/micron | 100 g/mil | ASTM D1709 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |