Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 0.276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.276 MPa
40.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.276 MPa
40.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-49 is manufactured using KEVLAR® 49 fabric. A thermosetting adhesive is used for the node bonds and a 350°F cure modified epoxy resin i..
Shear Strength >= 0.276 MPa
>= 40.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 0.276 MPa
>= 40.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.276 MPa
>= 40.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.276 MPa
>= 40.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.276 MPa
40.0 psi
2024 T3 Aluminum, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Shear Strength 0.276 - 0.414 MPa
40.0 - 60.0 psi
Overlap, Neoprene Rubber/Steel
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 0.276 - 0.414 MPa
40.0 - 60.0 psi
Overlap, Neoprene Rubber/Steel
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Copyright © lookpolymers.com All Rights Reserved