Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.393 MPa | >= 57.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 1/4-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.393 MPa | >= 57.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 3/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.393 MPa | >= 57.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 0.393 MPa | >= 57.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Cold Rolled Steel, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Polycarbonate, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Overlap, Fir, 50% RH |
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Overlap, Fir, 50% RH |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Overlap, Fir, 50% RH |
3M PN8027 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.393 MPa | 57.0 psi | Overlap, Fir, 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |