Polymer Property : Shear Strength = 0.552 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.552 MPa
80.0 psi
Plate Shear, W Direction
Hexcel® HexWeb® ACG®-1/2 Honeycomb Aluminum Commercial Grade
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. ..
Shear Strength 0.552 MPa
80.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.552 MPa
>= 80.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.552 MPa
80.0 psi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-78 - 1/4 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Shear Strength >= 0.552 MPa
>= 80.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 5/32-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.552 MPa
80.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.552 MPa
80.0 psi
Dow Corning SE 738 SILICONE RTV
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning
Shear Strength 0.552 MPa
80.0 psi
Overlap, Polypropylene
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
Shear Strength 0.552 - 0.689 MPa
80.0 - 100 psi
Overlap, SBR/Steel
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 0.552 MPa
80.0 psi
Overlap, Aluminum, 60°C for 30 mins; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 0.552 MPa
80.0 psi
Cohesion Dynamic, PET/Polycarbonate; ASTM D1002
3M 7953MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Shear Strength 0.552 MPa
80.0 psi
Overlap, Polypropylene
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
Shear Strength 0.552 MPa
80.0 psi
Dynamic Shear to Stainless Steel; ASTM D1002
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Shear Strength 0.552 MPa
80.0 psi
Dynamic Shear to Stainless Steel; ASTM D1002
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Shear Strength 0.552 MPa
80.0 psi
Dynamic Shear to Stainless Steel; ASTM D1002
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Shear Strength 0.552 - 0.689 MPa
80.0 - 100 psi
Overlap, SBR/Steel
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength >= 0.552 MPa
>= 80.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 3/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Copyright © lookpolymers.com All Rights Reserved