Mechanical Properties Metric English Comments
Shear Strength 0.883 MPa
128 psi
Plate Shear, L Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Shear Strength 0.883 MPa
128 psi
Plate Shear, W Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.5 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..