Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 1.86 MPa | >= 270 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 5/32-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 5/32-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, W Direction |
Hexcel® HexWeb® HRH-36 - 1/8 - 6.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP/OX - 3/8 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 1.86 MPa | >= 270 psi | Plate Shear, L Direction, min, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Designation: Material-Cell Size-Density.Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 1.86 MPa @Temperature 71.0 °C |
270 psi @Temperature 160 °F |
Overlap |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 1.86 MPa | 270 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 1.86 MPa | 270 psi | Overlap, HIPS (IPA/abrade/IPA)-Adhesive Failure; ASTM D1002 |
3M Scotch-Weld™ LSB90 Flexible Epoxy 3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife.. |
|||
Shear Strength | 1.86 MPa @Temperature 71.0 °C |
270 psi @Temperature 160 °F |
Overlap |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |