Mechanical Properties Metric English Comments
Shear Strength 80.0 MPa
11600 psi
ASTM D732
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Shear Strength 80.0 MPa
11600 psi
ASTM D732
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern.
Shear Strength 80.0 MPa
11600 psi
ASTM D732
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Shear Strength 80.0 MPa
11600 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Shear Strength 80.0 MPa

@Temperature 22.0 °C
11600 psi

@Temperature 71.6 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M60J Fiber
Information provided by HexCel
Shear Strength 80.0 MPa
11600 psi
0°, Short Beam
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2
Information provided by HexCel
Shear Strength 80.0 MPa
11600 psi
0°, Short Beam
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2
Information provided by HexCel
Shear Strength 80.0 MPa

@Temperature 22.0 °C
11600 psi

@Temperature 71.6 °F
Hexcel® HexPly® 954-3 Curing Cyanate Resin, M55J Fiber
Information provided by HexCel
Shear Strength 80.0 MPa
11600 psi
0°, Short Beam
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2
Information provided by HexCel
Shear Strength 80.0 MPa
11600 psi
In-Plane, RT, Dry; EN6031
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Shear Strength 80.0 - 90.0 MPa
11600 - 13100 psi
IS 867-1963
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
Shear Strength 80.0 MPa
11600 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..