Polymer Property : Shear Strength = 12500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 86.2 MPa

@Thickness 15.7 mm
12500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP424 Laminate
Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el..
Shear Strength 86.5 MPa
12500 psi
Interlaminar; 0° Fiber Direction; ASTM D2344
Saint-Gobain Quartzel® Fiber/Cyanate Ester Resin Unidirectional Composite
Fiber: Quartzel® Silica Roving C9 667 QS16 (33). Resin: YLA RS-3C.Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous,..
Shear Strength 86.0 MPa
12500 psi
ASTM D732
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.