Shear Strength 13.77 MPa
1997 psi
Lap
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy
Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic..