Polymer Property : Shear Strength = 35.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 35.0 MPa
5080 psi
0°, Short Beam
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2
Information provided by HexCel
Shear Strength 35.0 MPa

@Temperature 135 °C
5080 psi

@Temperature 275 °F
0º, ILSS Short Beam, Wet; EN2563
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Information provided by HexCel
Shear Strength 35.0 MPa

@Temperature 100 °C
5080 psi

@Temperature 212 °F
0º, ILSS (Short Beam), Wet; EN2563
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets
Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit I Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity.Application: Insulation material in hig..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Shear Strength 35.0 MPa
5080 psi
Cytec Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Shear Strength 35.0 MPa
5080 psi
Short Beam
Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite
Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec.
Shear Strength >= 35.0 MPa
>= 5080 psi
Parallel to laminations; IEC 1212-2 5.6
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe.
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr..
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha..