Mechanical Properties Metric English Comments
Shear Strength 55.0 - 62.1 MPa
7980 - 9000 psi
Average value: 59.7 MPa Grade Count:3
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Shear Strength 55.0 MPa
7980 psi
0°, Short Beam
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2
Information provided by HexCel
Shear Strength 55.0 MPa
7980 psi
0º, ILSS Short Beam, RT, Dry; EN2563
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber
Information provided by HexCel
Shear Strength 55.0 MPa

@Thickness >=5.00 mm
7980 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Shear Strength 55.0 MPa

@Thickness >=5.00 mm
7980 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t..
Shear Strength 55.0 MPa

@Thickness >=5.00 mm
7980 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Shear Strength 55.0 MPa

@Thickness >=5.00 mm
7980 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
Shear Strength 55.0 MPa
7980 psi
Cytec Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Shear Strength 55.0 MPa
7980 psi
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Shear Strength 55.0 MPa
7980 psi
ASTM D3846
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t..
Shear Strength 55.0 - 70.0 MPa
7980 - 10200 psi
IS 867-1963
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Ashley Polymers Ashlene® 180 Acetal
A general purpose, high viscosity, natural.Data provided by the manufacturer
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Ashley Polymers Ashlene® 190 Acetal
A general purpose, medium viscosity, natural.Data provided by the manufacturer
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Ashley Polymers Ashlene® 192-N2 Acetal
A general purpose, high viscosity, natural.Data provided by the manufacturer
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Ashley Polymers Ashlene® 195-N2 Acetal
A general purpose, medium viscosity natural.Data provided by the manufacturer
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Ashley Polymers Ashlene® 197-N2 Acetal
A general purpose, very low viscosity, in natural.Data provided by the manufacturer
Shear Strength 55.0 - 60.0 MPa
7980 - 8700 psi
IS 867-1963
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..