Polymer Property : Shear Strength = 71.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Shear Strength 71.0 MPa
10300 psi
IL; pr EN 2563
Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix
Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2Information provided by HexCel
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Shear Strength 71.0 MPa
10300 psi
Warp ILSS, RT
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26/45%/G1070 Carbon Fabric
6K T300J 370 gsmInformation provided by HexCel
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..