Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | IS 867-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |