Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 55.0 - 62.1 MPa | 7980 - 9000 psi | Average value: 59.7 MPa Grade Count:3 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Shear Strength | 55.0 MPa | 7980 psi | 0°, Short Beam |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2 Information provided by HexCel |
|||
Shear Strength | 55.0 MPa | 7980 psi | 0º, ILSS Short Beam, RT, Dry; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Shear Strength | 55.0 MPa @Thickness >=5.00 mm |
7980 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Shear Strength | 55.0 MPa @Thickness >=5.00 mm |
7980 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Shear Strength | 55.0 MPa @Thickness >=5.00 mm |
7980 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Shear Strength | 55.0 MPa @Thickness >=5.00 mm |
7980 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |
|||
Shear Strength | 55.0 MPa | 7980 psi | |
Cytec Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Shear Strength | 55.0 MPa | 7980 psi | |
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D3846 |
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t.. |
|||
Shear Strength | 55.0 - 70.0 MPa | 7980 - 10200 psi | IS 867-1963 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D732 |
Ashley Polymers Ashlene® 180 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D732 |
Ashley Polymers Ashlene® 190 Acetal A general purpose, medium viscosity, natural.Data provided by the manufacturer |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D732 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D732 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Shear Strength | 55.0 MPa | 7980 psi | ASTM D732 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Shear Strength | 55.0 - 60.0 MPa | 7980 - 8700 psi | IS 867-1963 |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |