Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 80.0 MPa | 11600 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Shear Strength | 80.0 MPa | 11600 psi | ASTM D732 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Shear Strength | 80.0 MPa | 11600 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Shear Strength | 80.0 MPa | 11600 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Shear Strength | 80.0 MPa @Temperature 22.0 °C |
11600 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M60J Fiber Information provided by HexCel |
|||
Shear Strength | 80.0 MPa | 11600 psi | 0°, Short Beam |
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2 Information provided by HexCel |
|||
Shear Strength | 80.0 MPa | 11600 psi | 0°, Short Beam |
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2 Information provided by HexCel |
|||
Shear Strength | 80.0 MPa @Temperature 22.0 °C |
11600 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Shear Strength | 80.0 MPa | 11600 psi | 0°, Short Beam |
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2 Information provided by HexCel |
|||
Shear Strength | 80.0 MPa | 11600 psi | In-Plane, RT, Dry; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Shear Strength | 80.0 - 90.0 MPa | 11600 - 13100 psi | IS 867-1963 |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
Shear Strength | 80.0 MPa | 11600 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |